Resumen

Se evaluó la biolixiviación en columnas, por fases inversas, para recuperar el hierro y cobalto, que están presentes en un relave minero urbano, abandonado.  En la biolixiviación se utilizaron dos micro columnas de polietileno, usando bacterias Acidithiobacillus ferrooxidans y Quimiolitotróficas nativas aisladas de las aguas del mismo humedal, para comparar su rendimiento frente a bacterias obtenidas en el laboratorio. Se recuperó un 20,7% de Fe, usando bacterias del laboratorio. Con las bacterias autóctonas se logró extraer un 0,06% de Fe. La extracción del Cobalto fue 21 ppm con bacterias de laboratorio y no se extrajo con bacterias nativas del humedal. Es factible extraer el Hierro del relave con biolixiviación, usando bacterias especialistas, con bacterias nativas del humedal la recuperación fue baja. Esta tecnología no permite recuperar el cobalto bajo las condiciones del estudio.

Abstract

Reverse-phase column bioleaching was evaluated to recover iron and cobalt present in an abandoned urban mine tailing. Two polyethylene micro columns were used in the bioleaching process, using native Acidithiobacillus ferrooxidans and Chemolithotrophic bacteria isolated from the waters of the same wetland, to compare their performance against bacteria obtained in the laboratory. 20.7% Fe was recovered, using bacteria from the laboratory. With the autochthonous bacteria, 0.06% of Fe was extracted. The Cobalt extraction was 21 ppm with laboratory bacteria and it was not extracted with native bacteria from the wetland. It is feasible to extract Iron from the tailing with bioleaching, using specialist bacteria, with native bacteria from the wetland the recovery was low. This technology does not allow the recovery of cobalt under the conditions of the study.

 

Palabras clave: relave minero, pasivo ambiental, biolixiviación, recuperación de elementos metálicos Keywords: mining tailings, environmental liabilities, bioleaching, recovery of metal elements


Dejar una respuesta

Tu dirección de correo electrónico no será publicada. Los campos obligatorios están marcados con *

Puedes usar estas etiquetas y atributos HTML:

<a href="" title=""> <abbr title=""> <acronym title=""> <b> <blockquote cite=""> <cite> <code> <del datetime=""> <em> <i> <q cite=""> <s> <strike> <strong>